Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 7.00 MPa @Strain 1 % |
1020 psi @Strain 1 % |
ISO 604 |
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data) By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey.. |
|||
Compressive Strength | 7.00 MPa @Strain 1 % |
1020 psi @Strain 1 % |
ISO 604 |
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data) TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion.. |
|||
Compressive Strength | 7.00 MPa @Strain 1 % |
1020 psi @Strain 1 % |
ISO 604 |
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
Compressive Strength | 7.00 MPa @Strain 1 % |
1020 psi @Strain 1 % |
ISO 604 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Compressive Strength | 7.00 MPa @Strain 1 % |
1020 psi @Strain 1 % |
ISO 604 |
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data) This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b.. |
|||
Compressive Strength | 7.00 MPa @Strain 1 % |
1020 psi @Strain 1 % |
ISO 604 |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Compressive Strength | 7.00 - 17.0 MPa @Temperature 1000 °C |
1020 - 2470 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 120 Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai.. |
|||
Compressive Strength | 7.00 - 13.0 MPa @Temperature 100 °C |
1020 - 1890 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 145 P Dense Refractory Castable Description: This material with an extreme plasticity is well suited for repair work or application as a thin layer.Remarks: These values apply to cast products.Information provided by Gouda Vuurvas.. |
|||
Compressive Strength | 7.00 - 13.0 MPa @Temperature 1400 °C |
1020 - 1890 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 145 P Dense Refractory Castable Description: This material with an extreme plasticity is well suited for repair work or application as a thin layer.Remarks: These values apply to cast products.Information provided by Gouda Vuurvas.. |
|||
Compressive Strength | 7.00 - 13.0 MPa @Temperature 1000 °C |
1020 - 1890 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p.. |
|||
Compressive Strength | 7.00 - 13.0 MPa @Temperature 1000 °C |
1020 - 1890 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al.. |