Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2.21 MPa @Treatment Temp. 540 °C |
320 psi @Treatment Temp. 1000 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Bazelite 2300 Insulating Castable Blaz 2300 is a lightweight, general purpose insulating castable. Can be used for back-up or exposed to furnace conditions. Used for one-shot linings, petrochemical heaters, combustion chambers and f.. |
|||
Compressive Strength | 2.21 MPa @Temperature 1095 °C |
320 psi @Temperature 2003 °F |
Cold Crush Strength |
BNZ Materials Bazelite 2300 LI Insulating Castable Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u.. |