Mechanical Properties Metric English Comments
Compressive Strength 2.21 MPa

@Treatment Temp. 540 °C
320 psi

@Treatment Temp. 1000 °F
Cold Crush Strength; Dried 104°C
BNZ Materials Bazelite 2300 Insulating Castable
Blaz 2300 is a lightweight, general purpose insulating castable. Can be used for back-up or exposed to furnace conditions. Used for one-shot linings, petrochemical heaters, combustion chambers and f..
Compressive Strength 2.21 MPa

@Temperature 1095 °C
320 psi

@Temperature 2003 °F
Cold Crush Strength
BNZ Materials Bazelite 2300 LI Insulating Castable
Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u..