Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2.90 MPa @Temperature 815 °C |
420 psi @Temperature 1500 °F |
|
BNZ Materials Bazelite 2000 Insulating Castable BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |
|||
Compressive Strength | 2.90 MPa @Temperature 1095 °C |
420 psi @Temperature 2003 °F |
Cold Crush Strength |
BNZ Materials Bazelite 2100 Insulating Castable Blaz 2100 is a general purpose lightweight castable for use as an exposed hot face refractory or as a very thermally efficient back-up to a dense refractory lining. Can be installed by casting, gunn.. |