Polymer Property : Compressive Strength = 420 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 2.90 MPa

@Temperature 815 °C
420 psi

@Temperature 1500 °F
BNZ Materials Bazelite 2000 Insulating Castable
BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i..
Compressive Strength 2.90 MPa

@Temperature 1095 °C
420 psi

@Temperature 2003 °F
Cold Crush Strength
BNZ Materials Bazelite 2100 Insulating Castable
Blaz 2100 is a general purpose lightweight castable for use as an exposed hot face refractory or as a very thermally efficient back-up to a dense refractory lining. Can be installed by casting, gunn..