Mechanical Properties Metric English Comments
Compressive Strength 1.96 - 2.94 MPa

@Temperature 1000 °C,
Time 10800 sec
284 - 427 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories DC-2BS Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 1.47 - 2.94 MPa

@Temperature 800 °C,
Time 10800 sec
213 - 427 psi

@Temperature 1470 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories GUN-100L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 1.47 - 2.94 MPa

@Temperature 1000 °C,
Time 10800 sec
213 - 427 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories GUN-110L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 1.47 - 2.94 MPa

@Temperature 500 °C,
Time 10800 sec
213 - 427 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories GUN-80L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 0.981 - 2.94 MPa

@Temperature 110 °C,
Time 86400 sec
142 - 427 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT-100S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 0.981 - 2.94 MPa

@Temperature 500 °C,
Time 10800 sec
142 - 427 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-100S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 0.981 - 2.94 MPa

@Temperature 500 °C,
Time 10800 sec
142 - 427 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-110S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 1.96 - 2.94 MPa

@Temperature 110 °C,
Time 86400 sec
284 - 427 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT-80N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).