Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.96 - 2.94 MPa @Temperature 1000 °C, Time 10800 sec |
284 - 427 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories DC-2BS Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 1.47 - 2.94 MPa @Temperature 800 °C, Time 10800 sec |
213 - 427 psi @Temperature 1470 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories GUN-100L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 1.47 - 2.94 MPa @Temperature 1000 °C, Time 10800 sec |
213 - 427 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories GUN-110L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 1.47 - 2.94 MPa @Temperature 500 °C, Time 10800 sec |
213 - 427 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories GUN-80L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 0.981 - 2.94 MPa @Temperature 110 °C, Time 86400 sec |
142 - 427 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-100S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 0.981 - 2.94 MPa @Temperature 500 °C, Time 10800 sec |
142 - 427 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-100S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 0.981 - 2.94 MPa @Temperature 500 °C, Time 10800 sec |
142 - 427 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-110S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 1.96 - 2.94 MPa @Temperature 110 °C, Time 86400 sec |
284 - 427 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-80N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |