Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Compressive Strength 1.96 - 2.94 MPa

@Temperature 1000 °C,
Time 10800 sec
284 - 427 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
2.94 - 4.90 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 711 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.349 W/m-K

@Temperature 260 °C
2.42 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.3722 W/m-K

@Temperature 540 °C
2.579 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.3955 W/m-K

@Temperature 800 °C
2.740 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
limited
Shrinkage -1.50 %

@Temperature 1000 °C,
Time 10800 sec
-1.50 %

@Temperature 1830 °F,
Time 3.00 hour
-0.0900 %

@Temperature 110 °C,
Time 86400 sec
-0.0900 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 35 %
35 %
SiO2 40 %
40 %
Descriptive Properties Value Comments
Installation Method Spray
Main Applications Corex
Material Required for Estimating (kg/?) 1,200
Water Required for Casting(%) 30-40