Mechanical Properties Metric English Comments
Compressive Strength 34.3 - 44.1 MPa

@Temperature 1350 °C,
Time 10800 sec
4980 - 6400 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-180G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 24.5 - 44.1 MPa

@Temperature 1500 °C,
Time 10800 sec
3560 - 6400 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories TPA-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).