Polymer Property : Compressive Modulus = 117.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 117.9 GPa

@Temperature 23.0 °C
17100 ksi

@Temperature 73.4 °F
Hexcel® F515 Epoxy Resin, TXX200 Carbon Tape
STD MOD FiberInformation provided by HexCel