Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 117.9 GPa @Temperature 23.0 °C |
17100 ksi @Temperature 73.4 °F |
|
Hexcel® F515 Epoxy Resin, TXX200 Carbon Tape STD MOD FiberInformation provided by HexCel |