Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 64.1 GPa @Temperature 21.1 °C |
9300 ksi @Temperature 70.0 °F |
Wet; ASTM D6641 |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-.. |
|||
Compressive Modulus | 64.1 GPa @Temperature 21.1 °C |
9300 ksi @Temperature 70.0 °F |
Dry, 90° Direction; ASTM D695 |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Compressive Modulus | 64.1 GPa @Temperature 24.0 °C |
9300 ksi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |
|||
Compressive Modulus | 64.1 GPa @Temperature 25.0 °C |
9300 ksi @Temperature 77.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |