Mechanical Properties Metric English Comments
Compressive Modulus 64.1 GPa

@Temperature 21.1 °C
9300 ksi

@Temperature 70.0 °F
Wet; ASTM D6641
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..
Compressive Modulus 64.1 GPa

@Temperature 21.1 °C
9300 ksi

@Temperature 70.0 °F
Dry, 90° Direction; ASTM D695
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric
Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures ..
Compressive Modulus 64.1 GPa

@Temperature 24.0 °C
9300 ksi

@Temperature 75.2 °F
Dry
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric
Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel
Compressive Modulus 64.1 GPa

@Temperature 25.0 °C
9300 ksi

@Temperature 77.0 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber
Information provided by HexCel