Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric

Category Polymer , Thermoset , Filled/Reinforced Thermoset
Manufacturer Renegade Materials Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-temp BMI’s, titanium and specialty metals. MVK-14 polyimide composites exhibit excellent mechanical and thermal properties in aerospace propulsion and airframe structure applications up to 600°F. MVK-14 is further supported by an FAA-conformed B-Basis Design-Allowable Database. MVK-14 Polyimide materials can be processed using autoclave or compression-molding. The product is available in fabric and unidirectional tape prepreg form, using carbon, quartz, ceramic and glass fibers.Information provided by Renegade Materials Corporation. Typical Properties for 14 mil CPT; autoclave cured at 600°F, with 625°F air post-cure.
Physical Properties Metric English Comments
Oxidative Stability 125 hour

@Temperature 316 °C,
Pressure 1.03 MPa
125 hour

@Temperature 600 °F,
Pressure 150 psi
<2% wt loss
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 827 MPa

@Temperature 21.1 °C
120000 psi

@Temperature 70.0 °F
Dry; ASTM D3039
841 MPa

@Temperature 288 °C
122000 psi

@Temperature 550 °F
Dry; ASTM D3039
848 MPa

@Temperature 232 °C
123000 psi

@Temperature 450 °F
Dry; ASTM D3039
Tensile Modulus 60.0 GPa

@Temperature 288 °C
8700 ksi

@Temperature 550 °F
Dry; ASTM D3039
61.4 GPa

@Temperature 21.1 °C
8900 ksi

@Temperature 70.0 °F
Dry; ASTM D3039
64.1 GPa

@Temperature 232 °C
9300 ksi

@Temperature 450 °F
Dry; ASTM D3039
Compressive Strength 262 MPa

@Temperature 288 °C
38000 psi

@Temperature 550 °F
Wet; ASTM D6641
345 MPa

@Temperature 232 °C
50000 psi

@Temperature 450 °F
Wet; ASTM D6641
379 MPa

@Temperature 288 °C
55000 psi

@Temperature 550 °F
Dry; ASTM D6641
483 MPa

@Temperature 232 °C
70000 psi

@Temperature 450 °F
Dry; ASTM D6641
607 MPa

@Temperature 21.1 °C
88000 psi

@Temperature 70.0 °F
Wet; ASTM D6641
731 MPa

@Temperature 21.1 °C
106000 psi

@Temperature 70.0 °F
Dry; ASTM D6641
Compressive Modulus 55.8 GPa

@Temperature 288 °C
8100 ksi

@Temperature 550 °F
Wet; ASTM D6641
59.3 GPa

@Temperature 232 °C
8600 ksi

@Temperature 450 °F
Wet; ASTM D6641
60.0 GPa

@Temperature 288 °C
8700 ksi

@Temperature 550 °F
Dry; ASTM D6641
61.4 GPa

@Temperature 21.1 °C
8900 ksi

@Temperature 70.0 °F
Dry; ASTM D6641
63.4 GPa

@Temperature 232 °C
9200 ksi

@Temperature 450 °F
Dry; ASTM D6641
64.1 GPa

@Temperature 21.1 °C
9300 ksi

@Temperature 70.0 °F
Wet; ASTM D6641
Shear Modulus 2.07 GPa

@Temperature 288 °C
300 ksi

@Temperature 550 °F
In-Plane, Dry; ASTM D790
2.76 GPa

@Temperature 232 °C
400 ksi

@Temperature 450 °F
In-Plane, Dry; ASTM D790
4.83 GPa

@Temperature 21.1 °C
700 ksi

@Temperature 70.0 °F
In-Plane, Dry; ASTM D790
Shear Strength 55.2 MPa

@Temperature 232 °C
8000 psi

@Temperature 450 °F
In-Plane, Dry; ASTM D790
62.1 MPa

@Temperature 288 °C
9000 psi

@Temperature 550 °F
In-Plane, Dry; ASTM D790
82.7 MPa

@Temperature 21.1 °C
12000 psi

@Temperature 70.0 °F
In-Plane, Dry; ASTM D790
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 274 °C
525 °F
Wet, Storage Modulus
318 °C
605 °F
Dry, Storage Modulus
Users viewing this material also viewed the following: