Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 59.3 GPa @Temperature 71.1 °C |
8600 ksi @Temperature 160 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 59.3 GPa @Temperature 93.3 °C |
8600 ksi @Temperature 200 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 59.3 GPa @Temperature 232 °C |
8600 ksi @Temperature 450 °F |
Wet; ASTM D6641 |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-.. |
|||
Compressive Modulus | 59.3 GPa @Temperature 210 °C |
8600 ksi @Temperature 410 °F |
Wet, 0° Direction; ASTM D6641 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Compressive Modulus | 59.3 GPa @Temperature 71.1 °C |
8600 ksi @Temperature 160 °F |
0°, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Compressive Modulus | 59.3 GPa @Temperature 71.0 °C |
8600 ksi @Temperature 160 °F |
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C) |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |