Zircar Ceramics AX Moldable Alumina-Silica Insulation

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Zircar Ceramics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Ceramics AX Moldable Alumina-Silica Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AX Moldable is a sticky fiber rich paste useful to obtain a hard surface coating, bond alumina-silica fiber based insulation products to themselves and to form complex shapes for use to 1260°C (2300°F).Information provided by Zircar Ceramics.
Physical Properties Metric English Comments
Bulk Density 0.800 g/cc
0.0289 lb/in³
Dry Density
Density 1.36 g/cc
0.0491 lb/in³
Wet Density
Solids Content 55 %
55 %
Loss On Ignition 5.0 %
5.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00276 GPa
0.400 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 0.0820 W/m-K

@Temperature 204 °C
0.569 BTU-in/hr-ft²-°F

@Temperature 399 °F
0.137 W/m-K

@Temperature 427 °C
0.951 BTU-in/hr-ft²-°F

@Temperature 801 °F
0.185 W/m-K

@Temperature 649 °C
1.28 BTU-in/hr-ft²-°F

@Temperature 1200 °F
0.221 W/m-K

@Temperature 871 °C
1.53 BTU-in/hr-ft²-°F

@Temperature 1600 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Shrinkage 4.00 %

@Temperature 1093 °C,
Time 86400 sec
4.00 %

@Temperature 1999 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Color White