Polymer Property : Izod Impact, Unnotched (ISO) = 22.4 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 47.0 kJ/m²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
Izod Impact, Unnotched (ISO) 47.0 kJ/m²

@Temperature 23.0 °C
22.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem ATX153R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 47.0 kJ/m²

@Temperature 23.0 °C
22.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched (ISO) 47.0 kJ/m²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Sax Polymers SAXAMID 226F5RY01 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5RY01 is a polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has a halogen-free flame retardant and UL listed.Information provided by SAX Polymers
Izod Impact, Unnotched (ISO) 47.0 kJ/m²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66
NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe..
Izod Impact, Unnotched (ISO) 47.0 kJ/m²

@Temperature 23.0 °C
22.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Izod Impact, Unnotched (ISO) 47.0 kJ/m²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid..