Mechanical Properties Metric English Comments
Peel Strength 0.351 kN/m

@Temperature -55.0 °C
2.00 pli

@Temperature -67.0 °F
Aluminum T-Peel; ASTM D1876
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Peel Strength 0.351 kN/m

@Temperature 82.0 °C
2.00 pli

@Temperature 180 °F
180°
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
Peel Strength 0.351 kN/m

@Temperature 66.0 °C
2.00 pli

@Temperature 151 °F
180°
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M