Peel Strength 0.701 kN/m

@Temperature 24.0 °C
4.00 pli

@Temperature 75.2 °F
Aluminum T-Peel; ASTM D1876
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Peel Strength 0.701 kN/m

@Temperature 82.0 °C
4.00 pli

@Temperature 180 °F
Aluminum T-Peel; ASTM D1876
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Peel Strength 0.701 kN/m

@Temperature -55.0 °C
4.00 pli

@Temperature -67.0 °F
Aluminum T-Peel; ASTM D1876
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Peel Strength 0.701 kN/m

@Temperature 24.0 °C
4.00 pli

@Temperature 75.2 °F
Aluminum T-Peel; ASTM D1876
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Peel Strength 0.701 kN/m

@Temperature 82.0 °C
4.00 pli

@Temperature 180 °F
Aluminum T-Peel; ASTM D1876
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Peel Strength 0.701 kN/m

@Temperature 24.0 °C
4.00 pli

@Temperature 75.2 °F
Aluminum T-Peel; ASTM D1876
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e..
Peel Strength 0.701 kN/m

@Temperature 82.0 °C
4.00 pli

@Temperature 180 °F
Aluminum T-Peel; ASTM D1876
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e..
Peel Strength 0.701 kN/m

@Temperature 14.0 °C,
Time 1.81e+6 sec
4.00 pli

@Temperature 57.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive
Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, ..
Peel Strength 0.701 kN/m

@Temperature 14.0 °C,
Time 1.81e+6 sec
4.00 pli

@Temperature 57.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive
Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, ..
Peel Strength 0.701 kN/m

@Temperature 66.0 °C
4.00 pli

@Temperature 151 °F
180°
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
Peel Strength 0.701 kN/m

@Temperature 23.0 °C
4.00 pli

@Temperature 73.4 °F
180° T-Peel, Nitrile/CRS
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Peel Strength 0.701 kN/m

@Temperature 107 °C
4.00 pli

@Temperature 225 °F
Adhesion on Aluminum; ASTM D3330
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Peel Strength 0.701 kN/m

@Temperature 107 °C
4.00 pli

@Temperature 225 °F
Adhesion on Aluminum; ASTM D3330
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Peel Strength 0.701 kN/m

@Temperature 150 °C
4.00 pli

@Temperature 302 °F
Adhesion on Aluminum; ASTM D3330
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Peel Strength 0.701 kN/m

@Temperature 150 °C
4.00 pli

@Temperature 302 °F
Adhesion on Aluminum; ASTM D3330
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Peel Strength 0.701 kN/m

@Temperature 82.0 °C
4.00 pli

@Temperature 180 °F
180°, Canvas/Steel
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive
Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov..
Peel Strength 0.701 kN/m

@Temperature 14.0 °C,
Time 1.81e+6 sec
4.00 pli

@Temperature 57.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive
Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, ..
Peel Strength 0.701 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
4.00 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1870 Industrial Adhesive
Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b..