Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL4019 PC Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | SABIC Method |
SABIC Innovative Plastics Lexan® FL933 PC Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized. |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL SE100X PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated FR resin. Improved productivity and reliability. 199F HDT. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 1285 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 1285 PEI (Asia Pacific) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRILOY D2000P PC (Asia Pacific) LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing. |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DD000P PC LNP* STAT-KON* DD000P is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East) Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea.. |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | ASTM Test |
Styrolution Luran® S 757 G ASA Luran S 757 G is an easy flowing injection molding ASA grade with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re.. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PX0844 PPE+PS PPE+PS blend. Unfilled. UL94 HB rated. Low water absorption. Hydrolytic stability. Dimensional stability. |
|||
Dart Drop, Total Energy | 40.0 J @Thickness 0.0500 mm |
29.5 ft-lb @Thickness 0.00197 in |
1300N; ISO 7765-2 |
Borealis Bormed™ RB801CF Polypropylene Random Copolymer Bormed™ RB801CF is a random copolymer. Applications: Bormed™ RB801CF is intended for packaging for medical devices, pouches, and packaging for pharmaceutical products. Additives: Bormed™ RB801C.. |
|||
Dart Drop, Total Energy | >= 40.0 J | >= 29.5 ft-lb | W<sub>501</sub> housing; ISO 6603-1 |
BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT Description: Is a PBT-HI, mineral-reinforced, impact-modified injection-molding grade for rigid parts, for example automotive power door locks.Information provided by BASF |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC (Asia Pacific) LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |