Mechanical Properties Metric English Comments
Falling Dart Impact 32.5 J

@Temperature -40.0 °C
24.0 ft-lb

@Temperature -40.0 °F
F50; ASTM D3029
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Falling Dart Impact 32.5 J
24.0 ft-lb
ASTM D3029
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Falling Dart Impact 32.5 J

@Temperature -40.0 °C
24.0 ft-lb

@Temperature -40.0 °F
F50; ASTM D3029
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Falling Dart Impact 32.5 J
24.0 ft-lb
ASTM D3029
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Falling Dart Impact 32.5 J

@Temperature -40.0 °C
24.0 ft-lb

@Temperature -40.0 °F
F50; ASTM D3029
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Falling Dart Impact 32.5 J
24.0 ft-lb
ASTM D3029
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Falling Dart Impact 32.5 J

@Temperature -40.0 °C
24.0 ft-lb

@Temperature -40.0 °F
F50; ASTM D3029
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Falling Dart Impact 32.5 J
24.0 ft-lb
ASTM D3029
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Falling Dart Impact 32.5 J

@Temperature -40.0 °C
24.0 ft-lb

@Temperature -40.0 °F
F50; ASTM D3029
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Falling Dart Impact 32.5 J
24.0 ft-lb
ASTM D3029
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Falling Dart Impact 32.5 J
24.0 ft-lb
ASTM D3029
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Falling Dart Impact 32.5 J

@Temperature -40.0 °C
24.0 ft-lb

@Temperature -40.0 °F
F50; ASTM D3029
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Copyright © lookpolymers.com All Rights Reserved