Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Impact Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of LP 551-01 include pails, housewares, heavy-duty crates, and industrial components. This resin meets FDA Regulation 21 CFR 177.1250, 3.1 and 3.2.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.953 g/cc
0.953 g/cc
ASTM D792
ESCR 100% Igepal® 5.0 hour
5.0 hour
Condition B; ASTM D1693
Melt Index of Compound 7.0 g/10 min
7.0 g/10 min
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM D2240
Tensile Strength, Yield 22.1 MPa
3200 psi
2"/min; ASTM D638
Elongation at Break 100 %
100 %
2"/min; ASTM D638
Flexural Modulus 0.896 GPa
130 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Falling Dart Impact 32.5 J

@Temperature -40.0 °C
24.0 ft-lb

@Temperature -40.0 °F
F50; ASTM D3029
Thermal Properties Metric English Comments
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746