Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 64.0 - 101 MPa
9280 - 14700 psi
Average value: 86.9 MPa Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
5 mm/min; parallel to flow; ASTM D638
Asahi Kasei Tenac® 5012 Acetal Homopolymer  (discontinued **)
Standard-flow grade, with reduced stiffness and increased elongation through addition of special polymers.Applications: Clips, fasteners, press-fit parts.This product is not a part of the standard p..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
5 mm/min; parallel to flow; ASTM D638
Asahi Kasei Tenac® LT805 Acetal Homopolymer, Low Friction Grade  (discontinued **)
Excellent friction and wear on metals.Applications: Keyboard parts, bearings for office machines, gears.This product is not a part of the standard product line dated 2003.
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM D638
Covestro Apec® DP9-9340R High-Heat Polycarbonate, Medical with Release  (discontinued **)
It is the responsibility of the medical device, biological product, or pharmaceutical manufacturer (Manufacturer) to determine the suitability of all component parts and raw materials, including the..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM D638
Covestro Apec® DP9-9341 High-Heat Polycarbonate, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM D638
Covestro Apec® DP9-9343 High-Heat Polycarbonate, UV Stabilized  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
DIN 53455; ASTM D638
Kolon Kopa® KN173HI Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
Tensile Strength, Ultimate 64.0 MPa

@Temperature 22.0 °C
9280 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP
SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM D638
Plenco 1586 Polyester, Pellet, Injection Molded
PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM D638
Plenco 5482 Phenolic, Granular, Injection Molded
PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM Data
Dow Tyril® 1011 SAN
TYRIL® 1011 SAN copolymer is a light stabilized general purpose injection molding resin available in crystone color only. It exhibits excellent weathering characteristics, high strength, good chemi..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ATSM D638
Ashley Polymers Ashlene® 1021 Polycarbonate
A general purpose injection molding grade, natural resin. Also available as: 1021R (with release), 1023 (with UV stabilizers); 1023R (with release and UV stabilizers).Data provided by the manufactu..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ATSM D638
Ashley Polymers Ashlene® 1641 Polycarbonate
A general purpose injection molding grade, natural resin, UL approved. Also available as: 1641R (with release); 1643 (with UV stabilizers); 1643R (with release and UV stabilizers).Data provided by ..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ATSM D638
Ashley Polymers Ashlene® P270WO PPO
An extrusion grade for high temperature applications requiring flame retardancy as well as high mechanical strength and toughness such as electrical housings.Data provided by the manufacturer
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ATSM D638
Ashley Polymers Ashlene® 1051 Polycarbonate
A general purpose injection molding grade, natural resin. Also available as: 1051R (with release), 1053 (with UV stabilizers), 1053R (with release and UV stabilizers).Data provided by the manufactu..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ATSM D638
Ashley Polymers Ashlene® 1503WO BK Polycarbonate
A rigid flame retardant polycarbonate, UV stabilized in black for applications requiring superior dimensional stability and overall toughness.Data provided by the manufacturer
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ATSM D638
Ashley Polymers Ashlene® 1621 Polycarbonate
A general purpose injection molding grade, natural resin, UL approved. Also available as: 1621R (with release); 1623 (with UV stabilizers); 1623R (with release and UV stabilizers).Data provided by ..
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM D651
Resinoid 1322 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ATSM D638
Ashley Polymers Ashlene® P270 PPO
An extrusion grade for high temperature applications as well as high mechanical strength and toughness such as electrical housings.Data provided by the manufacturer