Polymer Property : Tensile Strength, Ultimate = 102 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 102 - 200 MPa
14800 - 29000 psi
Average value: 148 MPa Grade Count:17
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an..
Tensile Strength, Ultimate 102 MPa
14800 psi
oriented film
Honeywell Aegis™ CSD High Barrier Nylon  (discontinued **)
Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw..
Tensile Strength, Ultimate 102 MPa
14800 psi
ASTM D638
Global PEI-110 Easy Flow, Polyetherimide
Information provided by Global Polymers Corporation.