Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 102 - 200 MPa | 14800 - 29000 psi | Average value: 148 MPa Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Tensile Strength, Ultimate | 102 MPa | 14800 psi | oriented film |
Honeywell Aegis™ CSD High Barrier Nylon
(discontinued **) Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw.. |
|||
Tensile Strength, Ultimate | 102 MPa | 14800 psi | ASTM D638 |
Global PEI-110 Easy Flow, Polyetherimide Information provided by Global Polymers Corporation. |