Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 620 - 750 MPa | 89900 - 109000 psi | Solution Annealed and Aged |
Materion Beryllium Copper Alloy 10C Castings (UNS C82000) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchTabul.. |
|||
Tensile Strength, Ultimate | 550 - 750 MPa | 79800 - 109000 psi | Minimum Guaranteed |
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |
|||
Tensile Strength, Ultimate | 662 - 752 MPa | 96000 - 109000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, Extra Spring 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | 650 - 750 MPa | 94300 - 109000 psi | Wire |
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Tensile Strength, Ultimate | 600 - 750 MPa | 87000 - 109000 psi | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, 2.5< diameter< 5 High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Tensile Strength, Ultimate | 650 - 750 MPa | 94300 - 109000 psi | Wire |
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |