Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
Pacific Sintered Materials FX-232-T Infiltrated High Carbon Steel Powdered Metal Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-50All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-50Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
Kennametal Stellite Tribaloy® 745 Age-hardened, highly alloyed, nickel base alloy in the casting form. Hardened by the presence of intermetallic compounds in the highly alloyed matrix. Unique combination of corrosion and wear resist.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical |
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical after Solution Annealing |
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in se.. |
|||
Tensile Strength, Ultimate | 600 MPa @Temperature 760 °C |
87000 psi @Temperature 1400 °F |
|
Haynes 25 alloy, cold worked sheet, 10% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Ultimate | 600 MPa @Temperature 760 °C |
87000 psi @Temperature 1400 °F |
|
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Annealed prior to test |
Special Metals INCOLOY® Alloy 330 A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospher.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Annealed |
Special Metals INCOLOY® Alloy 800 A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The.. |
|||
Tensile Strength, Ultimate | 600 - 700 MPa | 87000 - 102000 psi | |
SSAB Tunnplat Docol® 600DL High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact.. |
|||
Tensile Strength, Ultimate | 600 - 700 MPa | 87000 - 102000 psi | |
SSAB Tunnplat Docol® 600DP High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact.. |
|||
Tensile Strength, Ultimate | 600 - 700 MPa | 87000 - 102000 psi | |
SSAB Tunnplat Dogal 500YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
SSAB Tunnplat Domex® 034 BOR Rolled Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Ultimate | 600 - 760 MPa | 87000 - 110000 psi | |
SSAB Tunnplat Domex® 550MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
Universal Wire Works 308 Stainless Steel Electrode Universal 308 coated electrodes are used for welding unstabilized 18-8 stainless steels such as types 301, 302, 302B, 303, 308Se 304, 305, and 308. Universal 308 electrodes provide corrosion resista.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
Universal Wire Works 309 Stainless Steel Electrode Universal 309 electrodes are used for the welding of heat resisting type 309 stainless steel. Deposits retain strength and oxidation resistance up to 2000 degrees F. Typical applications include fur.. |
|||
Tensile Strength, Ultimate | 600 - 650 MPa | 87000 - 94300 psi | Rod |
CLAL-MSX ARCAP Anticorrosion AP4 H13 3/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Tensile Strength, Ultimate | >= 600 MPa | >= 87000 psi | |
CLAL-MSX NICLAL 3444 H14 4/4 Hard Copper Alloy, diameter < 8 Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |
|||
Tensile Strength, Ultimate | 600 - 700 MPa | 87000 - 102000 psi | |
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Tensile Strength, Ultimate | >= 600 MPa | >= 87000 psi | Rod |
CLAL-MSX ARCAP Anticorrosion AP1 H15 Spring, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical |
ATI Allegheny Ludlum Stainless Steel Ohmaloy® 40 Resistance Alloy Ohmaloy 40 alloy is a moderately magnetic, ductile stainless steel having extremely high electrical resistivity. In addition to imparting high electrical resistivity, the aluminum content in these .. |
|||
Tensile Strength, Ultimate | 600 - 700 MPa | 87000 - 102000 psi | |
ArcelorMittal Dual Phase 600 Very high strength steel, Cold Rolled Steel Available in the following: HCT780X (uncoated), HCT780X+ZE (electrogalvanized) and HCT780X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical; Annealed at 1800°F (982°C) |
ATI Allegheny Ludlum AL 800™ Nickel-Base Alloy, UNS N08800 AL 800 alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-corr.. |
|||
Tensile Strength, Ultimate | 600 - 700 MPa | 87000 - 102000 psi | |
ArcelorMittal Complex Phase Steel 600 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT600C) and electrogalvanized (HCT600C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC Allegheny Ludlum Type 420HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |
|||
Tensile Strength, Ultimate | 600 MPa @Temperature 400 °C |
87000 psi @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 904L High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |