Multibase Multi-Flex® TPE G 7455 X

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE G 7455 X.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex® G 7455 X is based on the Kraton G 78455 X formulation. It has low specific gravity as well as having a UL 94 rating of V-0. Ash is 5.2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.063 g/cc
0.03840 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0118 cm/cm
0.0118 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
10 sec; ASTM D-2240
Tensile Strength, Ultimate 11.6 MPa
1680 psi
ASTM D638
Elongation at Break 698 %
698 %
ASTM D638
Tear Strength 53.8 kN/m
307 pli
ASTM D624
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0