Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 11.9 MPa | 1730 psi | ASTM D638 |
Multibase Multi-Flex® TPE A 5009 Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 11.9 MPa | 1730 psi | |
Indium Corp. Indalloy® 1E In-Sn Solder Alloy Lowest melting point practical solder. Indium-tin eutectic with sharp melting point. Has good wettability on glass, quartz and many ceramics. Has good low temperature malleability and therefore com.. |
|||
Tensile Strength, Ultimate | 11.9 MPa | 1720 psi | |
Williams Advanced Alloys WS118 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 11.9 MPa @Treatment Temp. 150 °C, Time 605000 sec |
1720 psi @Treatment Temp. 302 °F, Time 168 hour |
Heat Aging; ASTM D 412/ASTM D 573 |
Zylog Neoplast® 180 FT EB Thermoplastic Vulcanizate Neoplast 180 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Tensile Strength, Ultimate | 11.9 MPa | 1730 psi | ASTM D638 |
Ecomass® 4703TU95 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Po.. |