Ecomass® 4703TU95 Tungsten Filled Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Ecomass Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 4703TU95 Tungsten Filled Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 11.0 g/cc
11.0 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.9 MPa
1730 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Tensile Modulus 0.668 GPa
96.9 ksi
ASTM D638
Flexural Strength 23.1 MPa
3350 psi
ASTM D790
Flexural Modulus 0.800 GPa
116 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 204 - 221 °C
400 - 430 °F
Mold Temperature 10.0 - 26.7 °C
50.0 - 80.0 °F
Drying Temperature 93.3 °C
200 °F
then reduce to 160°F
Dry Time 2 hour
2 hour
Users viewing this material also viewed the following: