Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 1230 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.48 MPa
1230 psi
post cured- 2 hours at 177°C
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.50 MPa
1230 psi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
Tensile Strength, Ultimate 8.48 MPa
1230 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 283-40MED Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..
Tensile Strength, Ultimate 8.48 - 80.0 MPa
1230 - 11600 psi
Average value: 16.6 MPa Grade Count:51
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Strength, Ultimate 8.48 MPa
1230 psi
post cured- 2 hours at 177°C; ASTM D412
Multibase C6-515 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.50 MPa
1230 psi
ISO 527-1/-2
DSM Arnitel® XG5855 TPC-ET
Extrusion Grade
Tensile Strength, Ultimate 8.48 MPa
1230 psi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 8.48 MPa
1230 psi
Dow Corning SILASTIC® LS 5-8720 FLUOROSILICONE RUBBER
20 Durometer, off-white, Fluorosilicone Base.Information provided by Dow Corning
Tensile Strength, Ultimate 8.50 MPa
1230 psi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 181-73 Thermoplastic Rubber  (discontinued **)
A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc..