Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 13.4 MPa | 1940 psi | ASTM D638-95 |
Multibase Multi-Pro® 5012 C Black 50% Filler Content Polypropylene Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 13.4 MPa | 1940 psi | |
Freudenberg Simrit V169 Fluoroelastomer Self-Lube Additives to elastomer compounds can improve the lubricity or non-stick performance of a seal. Specific compound ingredients may include fluoropolymer (TEFLON) additives, silicone additives or molyb.. |
|||
Tensile Strength, Ultimate | 13.4 MPa | 1950 psi | ASTM D638 |
Multibase Multi-Flex® 1047 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 13.4 MPa | 1950 psi | ASTM D638 |
Multibase Multi-Flex® A 9702 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Ultimate | 13.4 MPa | 1950 psi | ASTM D638 |
Multibase Multi-Flex® D 3804 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Tensile Strength, Ultimate | 13.4 MPa | 1950 psi | |
Sylvin Technologies 9077-90 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.4 MPa | 1950 psi | ASTM D638 |
Dow AMPLIFY™ EA 101 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 101 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |
|||
Tensile Strength, Ultimate | 13.4 MPa | 1940 psi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4725P General Purpose Molding FormulationNordel® IP 4725P |
|||
Tensile Strength, Ultimate | 13.4 MPa | 1950 psi | ASTM D638 |
Colorite Polymers 7884H General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |