Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® 1047 Black TPO Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyolefin
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® 1047 Black TPO Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.892 g/cc
0.892 g/cc
ASTM 792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Melt Flow 2.75 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.75 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 51
51
10 seconds; ASTM D2240
Tensile Strength, Ultimate 13.4 MPa
1950 psi
ASTM D638
Elongation at Break 650 %
650 %
ASTM D412
Flexural Modulus 0.414 GPa
60.0 ksi
1% Secant; ASTM D790
Tear Strength 99.9 kN/m
570 pli
ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -50.0 °C
-58.0 °F
ASTM D746
Flame Spread 13.4 mm/min
0.528 in/min
FM VSS-302
Descriptive Properties Value Comments
Fogging Min. 90
SAE-J275