Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 59.3 - 152 MPa
8600 - 22000 psi
Average value: 107 MPa Grade Count:102
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Tensile Strength, Ultimate 48.0 - 152 MPa
6960 - 22000 psi
Average value: 102 MPa Grade Count:73
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Tensile Strength, Ultimate 62.1 - 152 MPa
9000 - 22000 psi
Average value: 98.7 MPa Grade Count:27
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Tensile Strength, Ultimate 18.8 - 152 MPa
2730 - 22000 psi
Average value: 42.9 MPa Grade Count:18
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..