Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | ASTM D638 |
Nylene® 8100 Unfilled Nylon 6/12 Description: Nylene® 8100 is an unfilled specialty fiber. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation... |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | ASTM D638 |
Nylene® 9110 Unfilled Nylon 6/10 Description: Nylene® 9110 is an unfilled specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation... |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | ASTM D638 |
Nylene® Naxel™ PC1210 Polycarbonate Description: Naxel™ PC1210 is a 6 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources.. |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | ASTM D638 |
Nylene® Naxel™ PC45G FR 10% Glass Reinforced, Flame Retardant Polycarbonate Description: Naxel™ PC45G FR is a 10% glass fiber reinforced, flame retardant polycarbonate. PC45G FR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins ar.. |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9010 psi | ASTM Data |
Dow Isoplast® 202 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 202 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois.. |
|||
Tensile Strength, Ultimate | 62.1 - 152 MPa | 9000 - 22000 psi | Average value: 98.7 MPa Grade Count:27 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Tensile Strength, Ultimate | 62.1 - 105 MPa | 9000 - 15200 psi | Average value: 80.6 MPa Grade Count:8 |
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum .. |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | |
Hybrid Plastics Nanoreinforced® POSS® Polyimide Nanoreinforced® POSS® Polyimide is a hybrid nanocomposite that can serve as oxidation resistant and highly bondable form of polyimide. Upon exposure to oxidizing oxygen the POSS® polyimide .. |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | ASTM D638 |
Global PC-1403 Standard Grade Polycarbonate Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | ASTM D638 |
Global PC-1603 Standard Grade Polycarbonate Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 62.1 MPa @Thickness 3.17 mm |
9010 psi @Thickness 0.125 in |
|
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | ASTM D638 |
Techmer ES Electrafil® DB-50/SS/6/FR Polycarbonate, 6% Stainless Steel Fiber (dry blend), Flame Retardant |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | ASTM D412 |
Lubrizol Estane® AG 9550 Thermoplastic Polyurethane Type: Estane® AG 9550 is a polyether based aliphatic polyurethane designed for flat die extrusion into film and sheet products.Features: Very tough, high modulus, high tear and tensile properties t.. |
|||
Tensile Strength, Ultimate | 62.1 MPa @Temperature 760 °C |
9000 psi @Temperature 1400 °F |
|
Crucible Steel 416 Plus Chromium Steel Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4.. |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | ASTM D-638 |
CMT Materials REN Shape® 5169 Foundry Pattern Board REN SHAPE 5169 is an extremely tough, abrasion resistant board for use in CNC-machining foundry patterns, core boxes and other tools. It can be milled with hardened-steel cutters. The material has.. |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | |
AdvanSource Biomaterials ChronoFlex® AL 65D Biodurable Medical Grade Polyurethane ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas.. |
|||
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | |
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
Tensile Strength, Ultimate | 62.1 - 82.7 MPa | 9000 - 12000 psi | |
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil .. |
|||
Tensile Strength, Ultimate | 62.1 - 75.8 MPa | 9000 - 11000 psi | |
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers. |
|||
Tensile Strength, Ultimate | 62.1 - 82.7 MPa | 9000 - 12000 psi | |
Bulk Molding Compounds BMC 695 Vinyl Ester Molding Compound BMC 695 vinyl ester molding compound is a mineral filled glass fiber-reinforced vinyl ester compound suitable for compression and injection molding It is characterized by good moldability, oil and s.. |
|||
Tensile Strength, Ultimate | 62.1 - 228 MPa | 9000 - 33000 psi | Average value: 161 MPa Grade Count:37 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 62.1 - 115 MPa | 9000 - 16700 psi | Average value: 96.0 MPa Grade Count:12 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |