Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 112 MPa | 16200 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, at 50% RH
(dis AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Tensile Strength, Ultimate | 111.7 MPa | 16200 psi | ASTM D638 |
Plenco 51335 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51335 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in black only.Information .. |
|||
Tensile Strength, Ultimate | 112 - 195 MPa | 16200 - 28300 psi | Average value: 150 MPa Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Tensile Strength, Ultimate | 112 MPa | 16200 psi | ASTM D882 |
Honeywell Capran® 512 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 512 LL is a heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other high temperature .. |
|||
Tensile Strength, Ultimate | 112 MPa | 16200 psi | ASTM D882 |
Honeywell Capran® 518 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 518 LL is a green tinted, heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other hig.. |
|||
Tensile Strength, Ultimate | >= 112 MPa | >= 16200 psi | re-crystallized |
H.C. Starck Pure Niobium (Columbium) Applications: NRC® niobium metal is produced from electron beam melted ingots. Grain Stabilized Niobium (GSNb) is made by EB and VAR melting. Both materials are malleable, weldable, machineabl.. |
|||
Tensile Strength, Ultimate | 112 MPa | 16200 psi | ISO 527-1/-2 |
DSM Arnite® TV4 441 (PBT+PET)-GF20 20% Glass Reinforced |
|||
Tensile Strength, Ultimate | 112 MPa | 16200 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 633 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Tensile Strength, Ultimate | 112 MPa | 16200 psi | 5 mm/min |
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
Tensile Strength, Ultimate | 112 MPa | 16200 psi | 5 mm/min |
Arkema Group Rilsan® BZM 30 TL Nylon 11, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MHL,18-050,GF30Rigid grade with glass fiber (30%) filler for injection molding. Available colors: black and natural. Light and heat stabilized.Rigidity. High compressive st.. |
|||
Tensile Strength, Ultimate | 112 MPa | 16200 psi | ATSM D638 |
Ashley Polymers Ashlene® P266 PPO, 30% Glass Reinforced A general purpose, 30% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 112 MPa @Temperature 60.0 °C |
16200 psi @Temperature 140 °F |
ISO 527 |
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 112 MPa | 16200 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 756 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 112 MPa | 16200 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PI-10GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |