Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 19.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ISO 527
Polikim High Density Polyethylene (HDPE)
High density polyethylene is preferred when resistance to chemicals and weather is the priority. As it can be supplied in large dimensions and can be welded, its use in construction of tanks and was..
Tensile Strength, Ultimate 19.6 - 49.0 MPa
2840 - 7110 psi
Average value: 39.8 MPa Grade Count:29
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ASTM D638
Global J-1600 High Density Polyethylene
Description-suitable for injection moldingApplications-household products, handy craft flowers, toys, stationaryInformation provided by Global Polymers Corporation.
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ASTM D638
Global J-2308 High Density Polyethylene
Description-industrial injection grade w/ UV stabilizer, good for high impact strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided..
Tensile Strength, Ultimate 19.6 MPa
2840 psi
500mm/min; ASTM D638
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical
Tensile Strength, Ultimate 19.6 MPa
2840 psi
500mm/min; ASTM D638
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical
Tensile Strength, Ultimate 19.6 MPa
2840 psi
Shinil Chemical SHINNANO PP Polymer Nanocomposite Bumper
SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using..
Tensile Strength, Ultimate >= 19.6 MPa

@Temperature 100 °C
>= 2840 psi

@Temperature 212 °F
Sibur SKI-3 1st Grade, 2nd Group Isoprene Rubber (IR)
Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. For production of tires and rubber technical articles of wide assortment.
Tensile Strength, Ultimate >= 19.6 MPa

@Temperature 100 °C
>= 2840 psi

@Temperature 212 °F
Sibur SKI-3 1st Grade, 3rd Group Isoprene Rubber (IR)
Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. For production of tires and rubber technical articles of wide assortment.
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ASTM D412
SK Chemicals SKYTHANE® UB400 Hotmelt Lamination Film
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ASTM D412
Lubrizol Estane® T460A Thermoplastic Polyurethane
Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
Tensile Strength, Ultimate 19.6 MPa
2840 psi
500 mm/min; ASTM D 412
Zylog Neoplast® 240 FT EB Thermoplastic Vulcanizate
Neoplast 240 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro..
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ASTM D412
Lubrizol Estane® CR180A Thermoplastic Polyurethane
Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf..
Tensile Strength, Ultimate 19.6 MPa
2840 psi
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
DuPont Performance Polymers VTR 8525 (GBLT-S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued
FormulationVTR-8525
Tensile Strength, Ultimate 19.6 MPa
2840 psi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8655 (GBL-S) Peroxide Cured Fluoroelastomer (FKM)  (discontinued **)
FormulationVTR 8655
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ASTM D412
SK Chemicals SKYTHANE® 400 Hotmelt Grade UB Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ASTM D412
SK Chemicals SKYTHANE® 370A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Copyright © lookpolymers.com All Rights Reserved