Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 28.91 - 49.0 MPa

@Temperature 70.0 - 100 °C
4193 - 7110 psi

@Temperature 158 - 212 °F
Average value: 43.3 MPa Grade Count:1
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Tensile Strength, Ultimate 28.91 - 49.0 MPa

@Time 0.000 - 3.63e+6 sec
4193 - 7110 psi

@Time 0.000 - 1010 hour
Average value: 43.3 MPa Grade Count:1
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Tensile Strength, Ultimate 19.6 - 49.0 MPa
2840 - 7110 psi
Average value: 39.8 MPa Grade Count:29
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Tensile Strength, Ultimate 23.0 - 49.0 MPa
3340 - 7110 psi
Average value: 38.2 MPa Grade Count:25
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded