Polymer Property : Tensile Strength, Ultimate = 28.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 28.4 MPa
4120 psi
Vulcanized
KKPC KOSYN 1502G Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tensile Strength, Ultimate 28.4 MPa
4120 psi
150°C, 40 min., Pressure Vulcanization. -8% Change after 100°C, 70 hrs, Oil Immersion
KKPC KOSYN KNB 25LH Acrylonitrile Butadiene Rubber (NBR)
Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. ..
Tensile Strength, Ultimate 28.4 MPa
4120 psi
BCC Products Kwik Kast BC 8650 Urethane Casting
BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittl..