Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products Kwik Kast BC 8650 Urethane Casting

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer BCC Products
Trade Name Kwik Kast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products Kwik Kast BC 8650 Urethane Casting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittle parts. Designed for constructing patterns, prototypes, duplications, negatives, low temperature vacuum form tools, tracing models, etc.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.90 g/cc
1.90 g/cc
Brookfield Viscosity 2360 cP

@Temperature 23.9 °C
2360 cP

@Temperature 75.0 °F
1 minute
Linear Mold Shrinkage 0.00080 cm/cm
0.00080 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 81 - 85

@Temperature 23.9 °C
81 - 85

@Temperature 75.0 °F
Tensile Strength, Ultimate 28.4 MPa
4120 psi
Flexural Strength 43.1 MPa
6250 psi
Compressive Strength 63.4 MPa
9200 psi
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 24.0 °C
1.00 - 2.00 hour

@Temperature 75.2 °F
demold time
Pot Life 5.0 - 6.0 min

@Temperature 24.0 °C
5.0 - 6.0 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 1:1 by weight or volume
Users viewing this material also viewed the following: