Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 28.4 MPa | 4120 psi | Vulcanized |
KKPC KOSYN 1502G Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tensile Strength, Ultimate | 28.4 MPa | 4120 psi | 150°C, 40 min., Pressure Vulcanization. -8% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 25LH Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
Tensile Strength, Ultimate | 28.4 MPa | 4120 psi | |
BCC Products Kwik Kast BC 8650 Urethane Casting BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittl.. |