Tensile Strength, Ultimate 6.89 - 24.1 MPa
1000 - 3500 psi
Reinforced
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Nitrile Rubbers are copolymers of butadiene and acrylonitrile. The term has also been applied to copolymers of other dienes and/or nitriles. Acrylonitrile content may range from 18-50%. Increasin..
Tensile Strength, Ultimate 20.7 - 24.1 MPa
3000 - 3500 psi
TM R050-36
Resinlab® EP1305LV Black Epoxy Casting Resin
Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..
Tensile Strength, Ultimate 20.7 - 24.1 MPa
3000 - 3500 psi
TM R050-36
Resinlab® EP1305LV Clear Epoxy Casting Resin
Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..