Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Acetic acid vapors are released from the sealant surface as a by-product of cure.RTV106 sealant is a paste-consistency, standard strength high temperature sealant.Key Performance Properties: One-component productsCapability to cure at room temperature and ambient humiditySelf adhesion propertiesLow temperature flexibilityHigh temperature performanceExcellent weatherability and ozone and chemical resistanceExcellent electrical insulation propertiesApplications: Sealing heating elements, gasketing, electrical insulation, and other critical bonding and sealing applications where parts must perform at high temperatures. Can be applied to vertical or overhead surfaces.FDA 21 CFR 177.2600 USDA NSF International Std. No. 51GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Ultimate 2.55 MPa
370 psi
Elongation at Break 400 %
400 %
Adhesive Bond Strength 1.37 MPa
199 psi
At 100% cohesive failure
Tear Strength 6.86 kN/m
39.2 pli
Peel Strength 7.01 kN/m
40.0 pli
At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
Thermal Properties Metric English Comments
CTE, linear 270 µm/m-°C

@Temperature 20.0 °C
150 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
315 °C
599 °F
Intermittent
Brittleness Temperature -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+14 ohm-cm
3.00e+14 ohm-cm
Dielectric Constant 2.8

@Frequency 60 Hz
2.8

@Frequency 60 Hz
Dielectric Strength 20.0 kV/mm
508 kV/in
Dissipation Factor 0.0010

@Frequency 60 Hz
0.0010

@Frequency 60 Hz
Processing Properties Metric English Comments
Cure Time 20.0 min
0.333 hour
Tack-free
Descriptive Properties Value Comments
Application rate 400 g/min
Color Red
Consistency Paste
Users viewing this material also viewed the following: