Polymer Property : Tensile Strength, Ultimate = 41.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.6 - 41.4 MPa
4000 - 6000 psi
Average value: 34.4 MPa Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Strength, Ultimate 26.5 - 41.4 MPa
3840 - 6000 psi
Average value: 35.1 MPa Grade Count:4
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..
Tensile Strength, Ultimate 24.1 - 41.4 MPa
3500 - 6000 psi
ASTM D638
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Tensile Strength, Ultimate 27.6 - 41.4 MPa
4000 - 6000 psi
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP
BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is..
Tensile Strength, Ultimate 34.5 - 41.4 MPa
5000 - 6000 psi
Bulk Molding Compounds BMC 1403 Electrical Grade
BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo..
Tensile Strength, Ultimate 34.5 - 41.4 MPa
5000 - 6000 psi
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers
BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit..
Tensile Strength, Ultimate 34.5 - 41.4 MPa
5000 - 6000 psi
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was..
Tensile Strength, Ultimate 27.6 - 41.4 MPa
4000 - 6000 psi
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester
BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame..
Tensile Strength, Ultimate 27.6 - 41.4 MPa
4000 - 6000 psi
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester
BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda..
Tensile Strength, Ultimate 27.6 - 41.4 MPa
4000 - 6000 psi
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit..
Tensile Strength, Ultimate 34.5 - 41.4 MPa
5000 - 6000 psi
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound
BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..
Tensile Strength, Ultimate 27.6 - 41.4 MPa
4000 - 6000 psi
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade
BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne..
Tensile Strength, Ultimate 34.5 - 41.4 MPa
5000 - 6000 psi
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade
BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..
Tensile Strength, Ultimate 27.6 - 41.4 MPa
4000 - 6000 psi
ASTM D638
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..