Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 5.69 MPa | 825 psi | Silicone Property; ASTM D412 |
Arlon 32090R028 Silicone Rubber Laminate The interleave is 3 mil polyethylene, side 1 is uncured silicone rubber and the carrier is PET. |
|||
Tensile Strength, Ultimate | 5.69 MPa | 825 psi | silicone property; ASTM D412 |
Arlon 55096R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: uncured silicone rubber |
|||
Tensile Strength, Ultimate | 5.69 MPa | 825 psi | |
Momentive Performance Materials RTV630 Blue General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |