Material Notes:
The interleave is 3 mil polyethylene, side 1 is uncured silicone rubber and the carrier is PET.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
Silicone Property; Arlon SQA-TMS-024
Thickness 127 microns
5.00 mil
carrier; Arlon SQA-TMS-003
711 microns
28.0 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Silicone Property; ASTM D2240
Tensile Strength, Ultimate 5.69 MPa
825 psi
Silicone Property; ASTM D412
Elongation at Break 725 %
725 %
Silicone Property; ASTM D412
Tear Strength 28.6 kN/m
163 pli
Silicone Property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 31.3 kV/mm
794 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Red
Users viewing this material also viewed the following: