Polymer Property : Tensile Strength, Ultimate = 825 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5.69 MPa
825 psi
Silicone Property; ASTM D412
Arlon 32090R028 Silicone Rubber Laminate
The interleave is 3 mil polyethylene, side 1 is uncured silicone rubber and the carrier is PET.
Tensile Strength, Ultimate 5.69 MPa
825 psi
silicone property; ASTM D412
Arlon 55096R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: uncured silicone rubber
Tensile Strength, Ultimate 5.69 MPa
825 psi
Momentive Performance Materials RTV630 Blue General Purpose Potting/Encapsulating Compound
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..