Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.60 MPa | 1250 psi | |
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Uncured Carbon Black Filled Compound
& Carbon black compound with 100 parts Hypalon; 100 parts carbon black; 4 parts magnesia; and 1.5 parts propylene glycol. Physical property data below (except mooney viscosity) are for uncured film. .. |
|||
Tensile Strength, Ultimate | 8.60 MPa | 1250 psi | Compounded Tire |
Fluorosilicone Rubber (FMQ, FVMQ, FSi) Resists ozone and oxidizing chemicals, alkali, aromatic chlorinated solvents. Affected by brake fluid, ketones, and hydrazine. |
|||
Tensile Strength, Ultimate | 8.60 MPa | 1250 psi | |
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili.. |