Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | as molded |
Multibase SILASTIC® C7-4535 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 8.60 MPa | 1250 psi | |
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Uncured Carbon Black Filled Compound
& Carbon black compound with 100 parts Hypalon; 100 parts carbon black; 4 parts magnesia; and 1.5 parts propylene glycol. Physical property data below (except mooney viscosity) are for uncured film. .. |
|||
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Tensile Strength, Ultimate | 8.60 MPa | 1250 psi | Compounded Tire |
Fluorosilicone Rubber (FMQ, FVMQ, FSi) Resists ozone and oxidizing chemicals, alkali, aromatic chlorinated solvents. Affected by brake fluid, ketones, and hydrazine. |
|||
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | |
Sylvin Technologies 8960-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | |
Sylvin Technologies 8980-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | |
Sylvin Technologies 9077-75 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | |
Sylvin Technologies 9960-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | |
Sylvin Technologies 9980-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | |
Dow Corning S40 LIQUID SILICONE RUBBER KIT A heat-cured elastomer for use by customers fabricating medical devices, including those intended for implantation in humans for less than 30 days and non-implant applications. Dow Corning® S40 Liq.. |
|||
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | |
Cytec EN-2543 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Tensile Strength, Ultimate | 8.60 MPa | 1250 psi | |
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili.. |
|||
Tensile Strength, Ultimate | 8.62 MPa | 1250 psi | |
BCC Products MB 1300 Polyurethane Foam Modeling Board MB 1300 is a Mahogany colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1300 is medium low density foam of approximately 30lbs/ft3 board. Easily cut using CNC machining equi.. |