Polymer Property : Elmendorf Tear Strength TD = 210 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 210 g
210 g
ASTM D1922
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es..
Elmendorf Tear Strength TD 210 g
210 g
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli..
Elmendorf Tear Strength TD 210 g
210 g
ASTM D1922
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame..
Elmendorf Tear Strength TD 210 g
210 g
Dow LDPE 535I Low Density Polyethylene, Liner Grade
DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for..